中华人民共和国国家标准
(GB/T 7701.7-1997) 高效吸附用煤质颗粒活性炭
| 项 目 |
指标 |
| 优级品 |
一级品 |
| 孔容积,cm3/g |
≥0.80 |
| 比表面积,m2/g |
≥950 |
| 焦糖脱色率,% |
≥90 |
| pH值 |
6~10 |
| 水分,% |
≤5.0 |
| 强度,% |
≥85 |
| 碘吸附值,mg/g |
≥1050 |
1000~1049 |
| 四氯化碳吸附率,% |
≥80 |
70~79 |
| 灰分,% |
≤8 |
9~12 |
| 装填密度,g/L |
300~480 |
| 粒度,% |
φ1.5mm |
>2.50mm
|
≤2 |
| 1.25~2.50mm |
≥83 |
| 1.00~1.25mm |
<14 |
| <1.00mm |
≤1 |
| φ4.0mm |
>6.30mm
|
≤5 |
| 3.15~6.30mm |
≥90 |
| 2.50~3.15mm |
<4 |
| <2.50mm |
≤1 |